EN 10083-3  |  EN 10250-3  |  Quenched and Tempered Engineering Steel

A nickel-chromium-molybdenum alloy designed for heavy shafts, gears and forgings that need high strength, real toughness through the section, and predictable behavior after oil quenching and tempering.

  • Cr-Ni-Mo Low Alloy Steel
  • Material No. 1.6582
  • 28-34HRC Hardness
  • Bars and open-die forgings
  • QT:900-1200Mpa Tensile

What is 34CrNiMo6 Steel?

34CrNiMo6 is a quenched and tempered alloy engineering steel, registered under material number 1.6582. It is standardized in EN 10083-3 for bar products and in EN 10250-3 for open-die steel forgings.

The chemical composition of this steel primarily consists of approximately 1.5% nickel, 1.5% chromium, and 0.25% molybdenum, with a carbon content close to 0.34%.Nickel lifts toughness and hardenability, chromium supports hardenability and surface strength, and molybdenum helps the steel resist softening during tempering.The result is 34CrNiMo6 steel that reaches 900 to 1200 N/mm2 tensile strength in common engineering sections while keeping useful impact values, even at low temperatures.

Chemical Composition

GradeCMnPSSiCrNiMo
34CrNiMo6/1.65820.30-0.380.50-0.80≤0.025≤0.035≤0.41.3-1.71.3-1.70.15-0.3

Its strongest selling point is deep hardenability. On large round sections, the core hardens close to the surface rather than turning soft, which is why wind turbine main shafts and heavy transmission parts are so often specified in this grade.

However,34CrNiMo6 has only ordinary atmospheric corrosion resistance and will rust without paint, oil or another surface treatment. Weldability is limited because the alloy is sensitive to hardening and cracking in the heat-affected zone. It is also susceptible to temper embrittlement and to hydrogen flakes in large sections, both of which are controlled through correct heat treatment and verified testing rather than left to chance.

Where is 34CrNiMo6 Steel Used?

34CrNiMo6 steel is normally chosen for large, safety-relevant parts that carry repeated or shock loads rather than for simple brackets. Typical parts include:

  • Wind turbine main shafts and gearbox components, often in diameters above 300 mm
  • Crankshafts, camshafts, drive shafts, pump and worm shafts
  • Heavy gears, pinions, torsion bars and axle shafts
  • High-strength bolts, studs, tie rods and pins
  • Marine propeller shafts and rudder stocks
  • Aircraft landing gear and flap structural parts

34CrNiMo6 Steel Heat Treatment Basics

For 34CrNiMo6 steel, once the chemistry and section are fixed,the tempering temperature becomes the only effective means of balancing strength and toughness.Within the 540–680 °C window, hardness falls by roughly 0.5–1 HRC per 10 °C, which means a 40 °C change moves a part from a 320 HB wear-resistant condition to a 270 HB toughness-oriented one. Additionally, if possible, avoid high-temperature tempering within the temperature range of 350–550 °C. 34CrNiMo6 steel is prone to temper embrittlement within this temperature range.

34CrNiMo6+QT Mechanical properties per EN 10083-3

The following values ​​represent the performance requirements for 34CrNiMo6 after quenching and tempering according to EN 10083-3 standard.Note how quickly the guaranteed strength falls as the section grows: this is not a defect of the grade, it is a statement about how deeply it hardens in a given quench.

Section (mm)Rm (MPa)Re (MPa, min)A (%, min)Z (%, min)KV2 (J, min)
≤ 161,200–1,4001,000940By agreement
16–401,100–1,300900104545
40–1001,000–1,200800115045
100–160900–1,100700125545
160–250800–950600135545

34CrNiMo6+QT Mechanical properties per EN 10250-3

For open-die forgings to EN 10250-3 the structure of the requirement is different: strength levels are lower but impact is specified in both longitudinal and transverse directions, which is far more demanding than the bar table suggests.

Thickness (mm)Rm (MPa)Re (MPa)A (%, L / T)KV2 (J, L / T)
≤ 160≥ 800≥ 60013 / 945 / 22
160–330≥ 750≥ 54014 / 1045 / 22
330–660≥ 700≥ 49015 / 1140 / 20

In practice, a well-controlled Ø200 mm forged and Q&T bar can reach roughly 900–950 MPa tensile with 700–750 MPa yield, 17–18 % elongation and Charpy values above 100 J, at a hardness of about 300 HB. Those are typical achieved values, not guaranteed minimums. That gap between typical and guaranteed is why the purchase order must state the specimen location, test temperature and acceptance level.

34CrNiMo6 Steel Machining & Welding

Machining

Where the process route allows, 34CrNiMo6 should be machined in either the annealed (+A) or normalized (+N) state.At 248 HB maximum in the annealed state the steel cuts cleanly with carbide tooling and conventional speeds; in the Q&T condition at 300 HB or more, expect reduced tool life, higher cutting forces and a greater risk of surface damage on interrupted cuts.

If quenching is performed after machining, allowance should be made to remove deformation and decarburization. For thin-walled or asymmetrical parts, stress relief treatment should be performed before finishing.

Welding

The data doesn’t lie. There’s no doubt that 34CrNiMo6 steel has poor weldability and should not be used in welded structures.

If welding is unavoidable, preheating to 200–300 °C should be planned, a low-hydrogen welding process should be used, and post-weld heat treatment should be performed to eliminate residual stress. The welding process should be validated beforehand, as unheated welds on thick sections are highly susceptible to cracking.

34CrNiMo6 Steel vs. Other Deeper-Hardening Grades

Buyers often ask a more specific question than “Is 34CrNiMo6 steel good?”: “Is it worth the price?” The answer depends on section size and loading character.

GradeChemistry signaturePractical through-hardeningToughness and fatigueRelative cost
42CrMo40.38–0.45 C, 0.9–1.2 Cr, 0.15–0.3 Mo, no NiReliable to roughly Ø100–150 mm in oilAdequate; falls off quickly in thick sectionsBaseline
36CrNiMo40.32–0.40 C, 0.9–1.2 Cr, 0.9–1.2 NiRoughly Ø150–200 mmBetter than 42CrMo4, less than 34CrNiMo6+10–20 %
34CrNiMo60.30–0.38 C, 1.3–1.7 Cr, 1.3–1.7 Ni, 0.15–0.3 MoRoughly Ø250–300 mm with good oil quenching Best balance of strength and impact in this group+20–35 %
30CrNiMo80.26–0.34 C, 1.8–2.2 Cr, 1.8–2.2 NiBeyond Ø300 mmHighest hardenability; also highest embrittlement sensitivity+35–50 %

How to choose?

Choose 42CrMo4 when the section is under about 100 mm, the load is mainly bending or tension, and induction or nitriding hardening is available for the wear surfaces. It machines better and costs less.

Choose 34CrNiMo6 when the section exceeds 100 mm, when the part carries torque or reversing loads (shafts, crankshafts, gears), when specified strength is above 1,000 MPa with impact requirements attached, or when the design cannot tolerate a soft core.

Choose 30CrNiMo8 only when a Jominy curve or section test proves 34CrNiMo6 cannot reach the required core properties.

Frequently Asked Questions

Top FAQs for engineers and buyers choosing 34CrNiMo6 alloy steel. Can’t find your question? Reach out to our technical support team anytime.

What hardness does 34CrNiMo6 reach?2026-11-23T10:37:41+08:00
In the soft annealed condition,34CrNiMo6 is capped at 248 HB for machining. After quenching and tempering, measured hardness commonly sits around 280 to 330 HB, depending on section size and tempering temperature. Higher tempering points lower hardness while raising toughness, so the hardness should be specified together with the mechanical properties rather than on its own.
Is 34CrNiMo6 the same as AISI 4340?2026-11-21T15:44:44+08:00

Not exactly. They belong to the same Ni-Cr-Mo family and are often listed as equivalents, but their chemistry ranges differ and the standards do not automatically certify each other.

Dual certification is only possible when both analytical and testing results meet both specifications, and the heat treatment process still requires further verification.

What is the maximum section size for 34CrNiMo6?2026-09-02T16:56:10+08:00

34CrNiMo6 can be through-hardened in sections up to approximately 250 mm diameter when oil quenched. Beyond this size, the core cooling rate becomes insufficient for full martensitic transformation, and mechanical properties degrade toward the center.

For sections with a diameter greater than 250 mm, steel grades with higher hardenability should be considered, such as 30CrNiMo8 (1.6580).

How does 34CrNiMo6 compare to 18CrNiMo7-6 for gear applications?2026-09-02T16:53:06+08:00

These two grades serve different purposes. 34CrNiMo6 is a medium-carbon through-hardening steel used primarily for shafts and through-hardened gears, achieving 300–360 HB after QT. 18CrNiMo7-6 is a low-carbon carburizing grade designed for case-hardened gears — it produces a very hard wear-resistant case (58–62 HRC) with a tough, ductile core.

For wind turbine gearbox gears subject to high contact stresses and pitting risk, 18CrNiMo7-6 is generally preferred. For shafts, couplings, and gears where through-hardening is sufficient, 34CrNiMo6 is the more economical choice.

Is 34CrNiMo6 suitable for offshore wind turbines?2026-09-02T16:51:29+08:00

34CrNiMo6 is used in offshore wind turbine components, but it is not inherently corrosion-resistant. For offshore applications, components are protected by coatings (epoxy or polyurethane paint systems), grease, or sealed environments.

The grade’s primary advantage in offshore turbines is its mechanical performance,high fatigue strength and low-temperature toughness ,rather than corrosion resistance. Where components are directly exposed to salt spray, stainless steel or coated carbon steel is used for external surfaces, while 34CrNiMo6 remains the choice for internal load-bearing shafts.

What surface hardness can be achieved with induction hardening?2026-09-02T16:44:47+08:00

Induction hardening of 34CrNiMo6 typically produces surface hardness of 50–55 HRC, with case depths ranging from 2 to 8 mm depending on the induction frequency and power settings.

This is commonly applied to bearing journals, seal surfaces, and gear teeth. After induction hardening, a low-temperature temper at 150–200 °C is applied to relieve residual stresses without significantly reducing surface hardness.

Can 34CrNiMo6 be welded onto Wind turbine shafts?2026-09-02T15:38:31+08:00

Yes, but welding requires careful preheat and post-weld heat treatment due to the grade’s high carbon and alloy content, which makes it susceptible to cold cracking. Preheat to 200–300 °C, use low-hydrogen electrodes, and perform post-weld stress relieving at 600–650 °C.

For wind turbine main shafts, welding on the primary load path is generally avoided — the shaft is forged as a single piece. Welding is limited to non-critical attachments such as brackets or lifting lugs.

Is 34CrNiMo6 steel suitable for induction hardening?2026-01-20T20:57:19+08:00

34CrNiMo6 steel is suitable for induction hardening processes.

For 34CrNiMo6 steel, induction hardening is typically applied after an initial quenching and tempering treatment to establish a strong and tough core structure. The subsequent localized induction hardening, followed by low-temperature tempering, produces a deep hardened case with beneficial compressive residual stresses. This combination significantly enhances wear resistance and fatigue strength, making the process a preferred surface‑strengthening method for critical heavy‑duty components such as large gears and crankshafts.

What are the differences between 34CrNiMo6 steel and 42CrMo4 steel?2026-01-19T11:27:33+08:00

34CrNiMo6 and 42CrMo4 are both widely used high-strength alloy structural steels. Their core difference can be defined as the choice between performance and cost-effectiveness.

GradeCSiMnCrNiMoPS
42CrMo40.38-0.45≤ 0.40.6-0.90.9-1.2-0.15-0.3≤ 0.025≤ 0.035
34CrNiMo60.30-0.38≤ 0.40.5-0.81.3-1.71.3-1.70.15-0.3≤ 0.025≤ 0.035

The addition of nickel (Ni) makes 34CrNiMo6 surpass 42CrMo4 in terms of overall strength, toughness, and hardenability, but the cost also increases significantly.

How to choose?

34CrNiMo6: Maintains excellent strength and toughness even under extremely harsh conditions (large size, heavy impact, low temperature), offering the highest reliability.

42CrMo4: Capable of handling most high-load tasks, with balanced and reliable performance, and outstanding cost-effectiveness, making it an absolute “backbone” in the mechanical manufacturing field.Learn More

Is 34CrNiMo6 steel suitable for wind turbine main shafts?2026-01-19T09:45:33+08:00

34CrNiMo6 steel can be used to manufacture wind turbine main shafts.

34CrNiMo6, a high-hardenability alloy structural steel, delivers excellent strength-toughness balance and fatigue resistance after quenching and tempering. It is capable of withstanding the sustained alternating loads, torsional forces and impact loads acting on wind turbine main shafts during service, meeting the operational requirements of megawatt-class wind turbines and serving as a reliable material solution for wind turbine shaft manufacturing.Learn More

Is 34CrNiMo6 steel wear-resistant?2026-01-19T09:11:29+08:00

34CrNiMo6 steel is wear-resistant, but not the most wear-resistant.

As an alloy structural steel, the wear resistance of 34CrNiMo6 mainly comes from the high hardness/high strength after quenching and tempering heat treatment, which is sufficient to meet the conventional heavy-load, low-wear requirements of components such as gears and heavy-duty shafts.

The surface hardness of 34CrNiMo6 after quenching and tempering did not reach the high wear resistance level, which could not meet the stringent wear resistance requirements of high load and high friction. Therefore, it is necessary to add a surface strengthening process (surface quenching, nitriding) to further improve its surface hardness and wear resistance performance.

How to choose between 34CrNiMo6 and 30CrNiMo8?2026-01-18T16:47:41+08:00

Both 34CrNiMo6 and 30CrNiMo8 are high-strength alloy structural steels under the European standard system. As an upgraded version of 34CrNiMo6, the increased proportion of alloying elements in 30CrNiMo8 leads to a targeted improvement in performance:

  • Higher toughness: especially significantly improved low-temperature impact toughness and fracture toughness.
  • Stronger impact and fatigue resistance: better able to withstand sudden loads and repeated alternating stresses.
  • Better hardenability: enables the core of larger cross-section parts to achieve excellent mechanical properties after heat treatment.

Therefore, 34CrNiMo6, due to its excellent strength-toughness balance, is the most versatile high-strength alloy steel, fully meeting the needs of most conventional heavy-duty components. 30CrNiMo8, with its upgraded performance, is even more suitable for core components with larger cross-sections, higher loads, and extremely stringent safety and reliability requirements.Learn More

How to find a professional 34CrNiMo6 steel supplier?2026-01-17T11:06:28+08:00

Are you looking for a professional 34CrNiMo6 steel supplier in China?Whatever your answer may be, here at FUHONG we can help.

As Chinese First-Class Manufacturer, we focus on providing quality and new solutions for your needs in 34CrNiMo6. Thanks to modern technology and our professional team, you receive appropriate 34CrNiMo6 products for your company. Don’t hesitate to contact us in case you want to know how FUHONG can help your business .Learn More

Request a Quote for 34CrNiMo6

Send your drawing or specification and our technical team will come back with mill options, a delivery schedule and a firm price. The following details help us quote against the right standard the first time.
  • Dimensions and ruling section
  • Delivery condition (+A, +QT, bright)   
  • Required strength and hardness 
  • Charpy test temperature (room, -20 or -40 °C)   
  • Ultrasonic testing level 
  • Quantity and destination port
Send Your Inquiry
By |2026-11-23T10:48:08+08:00November 23rd, 2026|Steel Guide|0 Comments

Share This Article, Choose Your Platform!

Go to Top